水泥生料立式磨技術(shù)參數(shù)
| 型號(hào) |
PFRM53.4 |
PFRM38.4 |
PFRM36.4 |
PFRM34.4 |
PFRM32.4 |
PFRM28.3 |
PFRM27.3 |
PFRM25.2 |
PFRM22.2 |
PFRM17.2 |
PFRM14.2 |
| 磨盤直徑(mm) |
5300 |
3800 |
3600 |
3400 |
3200 |
2800 |
2700 |
2500 |
2200 |
1700 |
1400 |
| 磨輥個(gè)數(shù) |
4 |
4 |
4 |
4 |
4 |
3 |
3 |
2 |
2 |
2 |
2 |
| 裝機(jī)功率(kW) |
3600~4000 |
2000~2500 |
1800~2240 |
1600~1800 |
1400~1600 |
800~1250 |
800~1000 |
710~900 |
400~500 |
200~250 |
132~155 |
| 選粉機(jī)功率(kW) |
200 |
132 |
110 |
90 |
90 |
75 |
55 |
45 |
30 |
15 |
11 |
| 入磨大粒度(mm) |
≤100 |
≤85 |
≤80 |
≤70 |
≤70 |
≤70 |
≤65 |
≤70 |
≤50 |
≤40 |
≤40 |
| 入磨水份(%) |
6 |
6 |
6 |
6 |
6 |
6 |
6 |
6 |
6 |
6 |
6 |
| 出磨成品細(xì)度80μm篩余 (%) |
12~14 |
12~14 |
12~14 |
12~14 |
12~14 |
12~14 |
12~14 |
12~14 |
12~14 |
12~14 |
12~14 |
| 出磨成品水份 (%) |
0.5 |
0.5 |
0.5 |
0.5 |
0.5 |
0.5 |
0.5 |
0.5 |
0.5 |
0.5 |
0.5 |
| 原料易磨性指數(shù) (Wi) |
7.5~13 |
7.5~13 |
7.5~13 |
7.5~13 |
7.5~13 |
7.5~13 |
7.5~13 |
7.5~13 |
7.5~13 |
7.5~13 |
7.5~13 |
| 生產(chǎn)能力(t/h) |
330~510 |
185~280 |
170~260 |
140~210 |
125~190 |
85~130 |
78~120 |
60~90 |
40~65 |
22~33 |
13~20 |
桐乡市|
北流市|
云浮市|
嘉黎县|
宁陵县|
梁山县|
屯留县|
胶州市|
香河县|
霍山县|
高要市|
越西县|
二手房|
永新县|
涡阳县|
扎赉特旗|
天津市|
汤原县|
子长县|
武功县|
华亭县|
清镇市|
台北市|
鄂伦春自治旗|
普定县|
余庆县|
灵山县|
高碑店市|
车险|
三明市|
平遥县|
仁怀市|
枝江市|
乐亭县|
喀喇沁旗|
靖远县|
扶绥县|
阳信县|
东乌|
兴安盟|
县级市|